Most of the same stamps and skins used for freshly placed concrete can also be used to add pattern and texture to cement-based overlays. However, be careful not to purchase stamping mats with deep profiles that will exceed the overlay thickness.

Stamped overlays are typically applied at a thickness of 1/4 to 3/4 inch. As a general rule, the topping should be twice the thickness of the deepest pattern indent on the stamping mat. For example, if you plan to apply the overlay at a 1/2-inch thickness, don't buy a tool with an indent deeper than 1/4 inch. Generally, pattern depth won't be a problem with the thinner texturing skins.